China Clay for Paper Industry:

External or Free Iron impurities can be removed to an extent by Chemical Leaching method, however they cannot completely clean the kaolin from the free iron though this is the most efficient and aggressive method. Other reagents used for Fe removal from clay are pyrophosphate, oxalate, EDTA and CDB. The steps […]