Silicon Nitride Powder Preparation

Monday, July 13th, 2009

Carbothermic reduction of Silica
In this process Silica powder and Carbon powder is heated in a special furnace under nitrogen atmosphere a temperature of 1300 to 1700.C so as to form silicon monoxide. Which is react with nitrogen to form silicon nitride.
The unreacted carbon is removed by oxidation by heating at 500.C in air. In […]