Zirconia Powder Preparation
Tuesday, June 2nd, 2009Chlorination and Thermal Decomposition Method:
The naturally available Zircon and Carbon are mixed in a blender and then ground in an attritor mill for forming fine powder. The powder is then palatalized in a palatalizing machine. The pallets are then directly chlorinated at a temperature of 800oC to 1400oC in a shaft furnace or in a […]