DRYING OF CLAY MATERIALS
Friday, October 3rd, 2008In Brick manufacturing where the firing temperature is only 900oC to 1000oC maximum, the heat required for drying almost equals to the heat required for firing.
The mechanical strength of clay ware increases during drying and can be increased to the maximum extent by heating up to 300oC. The dry strength of clay increases with […]