Archive for May 27th, 2008

Casting (..contd)

Tuesday, May 27th, 2008

Thickened slip besides being difficult to pour and flow in the intricate parts of the mould can trap air bubbles giving pinholes in the cast. The casting time or slip holding time for earthenware body varies from 20 minutes to 40 minutes. The slip is poured into the mould left for casting to happen to […]