Preparation of Earthenware Body (..contd)

Tuesday, May 20th, 2008

In the next stage of the process the liquid ball clay slurry and the liquid china clay slurry are taken into a high speed blunger as per the batch formulation requirement. The silica is ground in a separate ball mill which is lined with silex stone and is then passed through a 200-mesh sieve and […]